Coreweld 80CNil is a metal cored wire designed for applications where good impact toughness is required.
| SKU | 243417052 |
|---|---|
| UPC | 662303076344 |
| Model / Product Description | CW 80C-NI1 052X600#OMP |
| Item Weight | 600.00 |
| Min Order | 1200 |
| Filler Metal Spec Def | |
| Size | .052 |
| Length | 600 in. |
| Weight | 600 lbs., Octagon Marathon Pack lbs. |
| Package | Octagon Marathon Pack |