ARCALOY MC409Ti

Arcaloy MC409Ti is a ferritic metal cored wire developed for welding similar ferritic steels requiring 11-12% Cr. The addition of Titanium (Ti) helps to optimized arc stability and improve weld metal transfer.

Ordering Information
SKU258076223
UPC662303074579
Model / Product DescriptionARC MC409TI 052X33#PSP
Item Weight33.00
Min Order33
Filler Metal Spec Def 
Size.052
Length33 in.
WeightSpool lbs., 33 lbs.
PackageSpool