Arcaloy 409Nb is a ferritic metal cored wire developed for welding similar ferritic steels requiring 11-12% Cr. The addition of Niobium (Nb) helps optimize weld metal transfer.
| SKU | 258080142 |
|---|---|
| UPC | 662303039226 |
| Model / Product Description | ARC 409NB 045X44#FSP |
| Item Weight | 44.00 |
| Min Order | 44 |
| Filler Metal Spec Def | |
| Size | .045 |
| Length | 44 in. |
| Weight | Spool lbs., 44 lbs. |
| Package | Spool |