ARCALOY 18CrCb

Arcaloy 18CrCb is a ferritic metal cored wire developed for welding similar ferritic steels requiring 18-19% Cr. The addition of Niobium (Nb) or Columbium (Cb) helps optimize weld metal transfer.

Ordering Information
SKU258076835
UPC662303069810
Model / Product DescriptionARC 18CRCB 045X600#OMP
Item Weight0.00
Min Order600
Filler Metal Spec Def 
Size.045
Weight0 lbs.
PackageOctagon Marathon Pack