Alloy Shield 410NiMo is a tubular, composite metal cored wire designed for welding CA-6NM castings or other similar Martensitic steels. Used in combination with 10.93 flux.
| SKU | 258078062 |
|---|---|
| UPC | 662303008864 |
| Model / Product Description | AS 410NIMO 1/8X500#POP |
| Item Weight | 500.00 |
| Min Order | 500 |
| Filler Metal Spec Def | |
| Size | 1/8 |
| Weight | 500 lbs. |
| Package | Pay Off Pack |