Arcaloy MC410 is a Martensitic metal cored wire for welding similar martensitic steels. Developed to maximize welding performance and reduce the cast to deposit.
| SKU | 258076108 |
|---|---|
| UPC | 662303054502 |
| Model / Product Description | ARC MC410 045X33#PSP |
| Item Weight | 33.00 |
| Min Order | 33 |
| Filler Metal Spec Def | |
| Size | .045 |
| Length | 33 in. |
| Weight | 33 lbs., Spool lbs. |
| Package | Spool |