Dual Shield II 70T-12H4 is an all-position, low hydrogen flux cored wire that provides excellent low temperature toughness. This flux cored wire provides a smooth arc and low spatter levels, excellent for construction, fabrication, offshore and railcar applications.
| SKU | 245016449 |
|---|---|
| UPC | 662303077853 |
| Model / Product Description | DS II 70T-12H4 1/16X600#OMP |
| Item Weight | 600.00 |
| Min Order | 1200 |
| Filler Metal Spec Def | |
| Size | 1/16 |
| Length | 600 in. |
| Weight | 600 lbs., Octagon Marathon Pack lbs. |
| Package | Octagon Marathon Pack |