DUAL SHIELD 7100 LC

Dual Shield 7100 LC is an all-position flux-cored wire for general purpose welding. It is tested and certified to meet the new AWS A5.20 ‘D’ designation requirements, making this gas-shielded wire an excellent choice for demand critical welds when FEMA 353, D1.1 or D1.8 Seismic Supplement is utilized.

Ordering Information
SKU248000945
UPC662303048099
Model / Product DescriptionDS 7100 LC 1/16X60#CL BK
Item Weight60.00
Min Order60
Filler Metal Spec Def 
Size1/16
Weight60 lbs.
PackageCoil Bulk Pack