DUAL SHIELD II 70 Ultra

Dual Shield II 70 Ultra is an all-position flux cored wire that displays exceptional impact properties in both as-welded and stress-relieved conditions.

Ordering Information
SKU245013313
UPC662303004491
Model / Product DescriptionDS II 70 ULT 045X33#PSP
Item Weight33.00
Min Order33
Filler Metal Spec Def 
Size.045
Length33 in.
Weight33 lbs., Spool lbs.
PackageSpool