DUAL SHIELD II 70 Ultra

Dual Shield II 70 Ultra is an all-position flux cored wire that displays exceptional impact properties in both as-welded and stress-relieved conditions.

Ordering Information
SKU245014626
UPC662303005443
Model / Product DescriptionDS II 70 ULT 035X10#FR HS
Item Weight10.00
Min Order50
Filler Metal Spec Def 
Size.035
Weight10 lbs.
PackageSpool