DUAL SHIELD 7000

Dual Shield 7000 is the industry's first all position flux cored wire combines excellent performance features with the ability to produce high quality welds.

Ordering Information
SKU245021324
UPC662303079277
Model / Product DescriptionDS 7000 045X600#OMP
Item Weight600.00
Min Order1200
Filler Metal Spec Def 
Size.045
Weight600 lbs.
PackageOctagon Marathon Pack