Print this page

DUAL SHIELD 111-RB

Dual Shield 111-RB is a low slag, high deposition flux cored electrode designed for joining structural components made of low carbon steel. It is good over rust and primer.

Ordering Information
SKU242215028
UPC662303080181
Model / Product DescriptionDS 111-RB 1/16X15#PSP
Item Weight15.00
Min Order60
Filler Metal Spec Def 
Size1/16
Length15 in.
Weight15 lbs., Spool lbs.
PackageSpool