Dual Shield Arc 70 is a large diameter flux cored wire for flat and horizontal welding over heavy rust and mill scale.
| SKU | 245002027 |
|---|---|
| UPC | 662303003692 |
| Model / Product Description | DS ARC-70 3/32X60#CL |
| Item Weight | 60.00 |
| Min Order | 60 |
| Filler Metal Spec Def | |
| Size | 3/32 |
| Length | 60 in. |
| Weight | 60 lbs., Coil lbs. |
| Package | Coil |