Dual Shield 8000-B2L is an all-position flux-cored wire for low carbon grades of 1. Cr - 0.5% Mo steels.
| SKU | 245005616 |
|---|---|
| UPC | 662303076863 |
| Model / Product Description | DS 8000-B2L 045X10#PSP VP |
| Item Weight | 10.00 |
| Min Order | 10 |
| Filler Metal Spec Def | |
| Size | .045 |
| Weight | 10 lbs. |
| Package | Spool |