DUAL SHIELD 8000-B2L

Dual Shield 8000-B2L is an all-position flux-cored wire for low carbon grades of 1. Cr - 0.5% Mo steels.

Ordering Information
SKU245006531
UPC662303037147
Model / Product DescriptionDS 8000-B2L 045X33#PSP VP
Item Weight33.00
Min Order33
Filler Metal Spec Def 
Size.045
Length33 in.
Weight33 lbs., Spool lbs.
PackageSpool