DUAL SHIELD 9000-C1

Dual Shield 9000-C1 is an all-position flux-cored wire which produces a 2.5% Ni deposit.

Ordering Information
SKU245012703
UPC662303004170
Model / Product DescriptionDS 9000-C1 1/16X33#AWS
Item Weight33.00
Min Order33
Filler Metal Spec Def 
Size1/16
Weight33 lbs.
PackageSpool