Dual Shield II 80-Ni1H4 is an all position low-hydrogen welding wire that provides excellent low temperature toughness in both the as welded and/or stress relieved conditions when used with 75% Ar / 25% CO2. It is tested and certified to meet the new AWS A5.20 ‘D’ designation requirements, making this gas-shielded wire an excellent choice for demand critical welds when FEMA 353, D1.1 or D1.8 Seismic Supplement is utilized.
| SKU | 245011630 |
|---|---|
| UPC | 662303058890 |
| Model / Product Description | DS II 80-NI1H4 1/16X60#CL |
| Item Weight | 60.00 |
| Min Order | 60 |
| Filler Metal Spec Def | |
| Size | 1/16 |
| Length | 60 in. |
| Weight | 60 lbs., Coil lbs. |
| Package | Coil |
All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.