Dual Shield II 101H4M was developed to meet the stringent requirements of MIL-E-24403/2 and offshore welding, and it is an ideal choice for HSLA steels.
| SKU | 245016456 |
|---|---|
| UPC | 662303078454 |
| Model / Product Description | DS II 101H4M 1/16X33#AWS VP |
| Item Weight | 33.00 |
| Min Order | 33 |
| Filler Metal Spec Def | |
| Size | 1/16 |
| Length | 33 in. |
| Weight | 33 lbs., Spool lbs. |
| Package | Spool |