Shield-Bright 309L X-tra was developed to maximize performance in the flat and horizontal positions when joining stainless to mild or carbon steel.
| SKU | 252201652 |
|---|---|
| UPC | 662303052881 |
| Model / Product Description | SBX 309L 1/16X33#PSP VP |
| Item Weight | 33.00 |
| Min Order | 33 |
| Filler Metal Spec Def | |
| Size | 1/16 |
| Length | 33 in. |
| Weight | 33 lbs., Spool lbs. |
| Package | Spool |