SHIELD-BRIGHT 309L X-tra

Shield-Bright 309L X-tra was developed to maximize performance in the flat and horizontal positions when joining stainless to mild or carbon steel.

Ordering Information
SKU252202643
UPC662303055059
Model / Product DescriptionSBX 309L 045X10#PSP VP/60CT
Item Weight10.00
Min Order10
Filler Metal Spec Def 
Size.045
Weight10 lbs.
PackageSpool