Cryo-Shield 308L is an all-position stainless steel cored wire designed for low temperature cryogenic applications.
| SKU | 252210000 |
|---|---|
| UPC | 662303034832 |
| Model / Product Description | CRYO-SH 308L 045X33#PSP VP |
| Item Weight | 33.00 |
| Min Order | 33 |
| Filler Metal Spec Def | |
| Size | .045 |
| Length | 33 in. |
| Weight | 33 lbs., Spool lbs. |
| Package | Spool |