CORESHIELD 8

Coreshield 8 is a self-shielded flux cored wire designed to weld critical structural applications while maintaining excellent arc characteristics and high welder appeal. Coreshield 8 is tested and certified to meet the new AWS D designation requirements, making this self-shielded wire an excellent choice for demand critical welds when the AWS D1.8 Seismic Supplement is utilized.

Ordering Information
SKU242206753
UPC662303081577
Model / Product DescriptionCS 8 072X20#AWS VP FEMA
Item Weight20.00
Min Order20
Filler Metal Spec Def 
Size.072
Length20 in.
Weight20 lbs., Spool lbs.
PackageSpool

All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.