CORESHIELD 8

Coreshield 8 is a self-shielded flux cored wire designed to weld critical structural applications while maintaining excellent arc characteristics and high welder appeal. Coreshield 8 is tested and certified to meet the new AWS D designation requirements, making this self-shielded wire an excellent choice for demand critical welds when the AWS D1.8 Seismic Supplement is utilized.

Ordering Information
SKU242206431
UPC662303072209
Model / Product DescriptionCS 8 5/64X22#AWS VP
Item Weight22.00
Min Order22
Filler Metal Spec Def 
Size5/64
Weight22 lbs.
PackageSpool