CORESHIELD 7

Coreshield 7 flux cored wire is a self-shielded wire designed for single or multiple pass welding of mild steel when impact toughness is not a requirement. Ideally suited for structural steel applications.

Ordering Information
SKU242202737
UPC662303001247
Model / Product DescriptionCS 7 1/16X50#CL
Item Weight50.00
Min Order50
Filler Metal Spec Def 
Size1/16
Weight50 lbs.
PackageCoil