CORESHIELD 40

Coreshield 40 is a self-shielded flux cored wire primarily designed for multiple pass, horizontal and flat position welding of low and medium carbon steels when toughness is not a requirement.

Ordering Information
SKU242201002
UPC662303000271
Model / Product DescriptionCS 40 3/32X50#CL
Item Weight50.00
Min Order50
Filler Metal Spec Def 
Size3/32
Length50 in.
Weight50 lbs., Coil lbs.
PackageCoil