Core-Bright 309L was developed for flat and horizontal welding without the use of a shielding gas when cladding or joining stainless to mild carbon steels.
| SKU | 258077163 |
|---|---|
| UPC | 662303054465 |
| Model / Product Description | CB 309L 045X33#PSP VP |
| Item Weight | 33.00 |
| Min Order | 33 |
| Filler Metal Spec Def | |
| Size | .045 |
| Length | 33 in. |
| Weight | 33 lbs., Spool lbs. |
| Package | Spool |