ALL-STATE SILFLO 15

A self-fluxing brazing alloy for copper to copper joining. Use for higher ductility in joints where close fit-up is impossible (.002" to .006") and electrical conductivity is important. Do not use with ferrous metals. For best result use with All-State S-200 or No.110 when joining copper to brass or bronze.