ALL-STATE SILFLO 0

A self-fluxing brazing alloy for copper to copper joining. For tight fitting joints (.001" to .002"). Do not use with ferrous metals. For best results use with All-State S-200 or No. 110 flux when joining copper to brass or bronze.

Ordering Information
SKU69060030
UPC662393003473
Model / Product DescriptionA/S SILFO 0 1/16X36X10X60
Item Weight0.00
Min Order10
Filler Metal Spec Def 
Size1/16
Length36 in.
Weight0 lbs.
PackageTube