Print this page

ALL-STATE 312

For welding high tensile alloys to high temperature heat-resisting alloys turbo-jet engines. Also for high yield steels, abrasion resisting steels and dissimilar steels. Weld deposit has the highest tensile and yield strength of any stainless electrode commonly in use.

Ordering Information
SKU69605112
UPC662393008980
Model / Product DescriptionA/S *312 1/16X36X10X60
Item Weight0.00
Min Order10
Filler Metal Spec Def 
Size1/16
Length36 in.
Weight0 lbs.
PackageTube

All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.