A bare rod for braze welding on steel pipe, plates and structural shapes in 50-60 ksi range and castings.
| SKU | 69703203 |
|---|---|
| UPC | 662393667781 |
| Model / Product Description | A/S RG-60 3/32X36X1# TUBE |
| Item Weight | 0.00 |
| Min Order | 1 |
| Filler Metal Spec Def | |
| Size | 3/32 |
| Length | 36 in. |
| Weight | 0 lbs. |
| Package | Tube |