ALL-STATE Chamfer Rod

Electrode for high speed chamfering, gouging, veeing out and beveling or any other metal removal.

Ordering Information
SKU69010130
UPC662393000588
Model / Product DescriptionA/S CHAMFER ROD 1/8X14X50CTN
Item Weight0.00
Min Order50
Filler Metal Spec Def 
Size1/8
Length14 in.
Weight50 lbs.
PackageCarton