Refrac-T-Back

Refrac-T-Back is a non-metallic ceramic material which is temporarily attached to the reverse side of a weld while helping to support a full penetration weld.

Ordering Information
SKU693000291
UPC662303042868
Model / Product DescriptionRTB FBF 1X1X1/4 36/CT
Item Weight0.00
Min Order1
Filler Metal Spec Def 
Size1/4 , 1
Length1 in., 0 in.
Weight0 lbs., Carton lbs.
PackageCarton