ALL-STATE LFB BARE

General Purpose Brazing rod.

Ordering Information
SKU69060001
UPC662303667788
Model / Product DescriptionA/S LFB BARE 3/32X36X50
Item Weight0.00
Min Order50
Filler Metal Spec Def 
Size3/32
Length36 in.
Weight0 lbs.