Atom Arc 8018-NM electrodes are used for welding the quenched and tempered manganese-molybdenum-nickel steels.
| SKU | 255205320 |
|---|---|
| UPC | 662303078027 |
| Model / Product Description | AA 8018-NM 5/32X18X50#HS |
| Item Weight | 50.00 |
| Min Order | 50 |
| Filler Metal Spec Def | |
| Size | 5/32 |
| Length | 18 in. |
| Weight | 50 lbs. |
| Package | Hermetically Sealed Can |