OK Autrod 13.20SC is designed to produce a 2-1/4% Cr and 1% Mo weld deposit to be used for welding process piping, heat exchangers, and pressure vessel fabrication. Used in combination with OK Flux 10.63 it meets step-cooling requirements.
| SKU | 2554F32 |
|---|---|
| UPC | 662303081775 |
| Model / Product Description | OK AUTROD 13.20SC 1/8X65#CL |
| Item Weight | 65.00 |
| Min Order | 65 |
| Filler Metal Spec Def | |
| Size | 1/8 |
| Length | 65 in. |
| Weight | 65 lbs., Coil lbs. |
| Package | Coil |