Spoolarc 29S is a general purpose wire suitable for many MIG and submerged arc carbon steel welding applications. Suitable for use over light rust.
| SKU | 1314F27 |
|---|---|
| UPC | 662303506667 |
| Model / Product Description | 29S 045X65#CL |
| Item Weight | 65.00 |
| Min Order | 65 |
| Filler Metal Spec Def | |
| Size | .045 |
| Length | 65 in. |
| Weight | 65 lbs., Coil lbs. |
| Package | Coil |