SPOOLARC 29S

Spoolarc 29S is a general purpose wire suitable for many MIG and submerged arc carbon steel welding applications. Suitable for use over light rust.

Ordering Information
SKU1315F67
UPC662303520571
Model / Product Description29S 045X1000#WFRL 80-100 5 AR
Item Weight1,000.00
Min Order1000
Filler Metal Spec Def 
Size.045
Weight1000 lbs., Reel lbs.
PackageReel