SPOOLARC 29S

Spoolarc 29S is a general purpose wire suitable for many MIG and submerged arc carbon steel welding applications. Suitable for use over light rust.

Ordering Information
SKU1316F10
UPC662303506810
Model / Product Description29S 3/32X800#DR
Item Weight800.00
Min Order1600
Filler Metal Spec Def 
Size3/32
Weight800 lbs.
PackageDrum