SPOOLARC 29S

Spoolarc 29S is a general purpose wire suitable for many MIG and submerged arc carbon steel welding applications. Suitable for use over light rust.

Ordering Information
SKU1319F05
UPC662303507121
Model / Product Description29S 035X500#MP
Item Weight500.00
Min Order1000
Filler Metal Spec Def 
Size.035
Length500 in.
Weight500 lbs., Marathon Pack lbs.
PackageMarathon Pack