Print this page

SPOOLARC 86

Spoolarc 86 contains higher levels of manganese and silicon than other grades of MIG wire. It provides a highly fluid puddle and excellent tolerance of rust and scale.

Ordering Information
SKU12Y9F85
UPC662303520175
Model / Product Description86 035X500#MP PBPLT
Item Weight500.00
Min Order1000
Size.035
Weight1000 lbs.