SPOOLARC 86

Spoolarc 86 contains higher levels of manganese and silicon than other grades of MIG wire. It provides a highly fluid puddle and excellent tolerance of rust and scale.

Ordering Information
SKU1382F08
UPC662303507961
Model / Product Description86 1/16X44#SP
Item Weight44.00
Min Order44
Filler Metal Spec Def 
Size1/16
Length44 in.
Weight44 lbs., Spool lbs.
PackageSpool