SPOOLARC 86

Spoolarc 86 contains higher levels of manganese and silicon than other grades of MIG wire. It provides a highly fluid puddle and excellent tolerance of rust and scale.

Ordering Information
SKU1382F84
UPC662303668044
Model / Product Description86 030X2#SP RANDOM WOUND
Item Weight2.00
Min Order2
Size.030
Weight2 lbs.