Spoolarc 95 is Military grade high strength wire used to weld HY-80 steels.
| SKU | 229DF28 |
|---|---|
| UPC | 000000000000 |
| Model / Product Description | 95 CU 1/16X36 F2 MIL |
| Item Weight | 15.00 |
| Min Order | 15 |
| Filler Metal Spec Def | |
| Size | 1/16 |
| Length | 36 in. |
| Weight | 15 lbs. |
| Package | Carton |