SPOOLARC 95

Spoolarc 95 is Military grade high strength wire used to weld HY-80 steels.

Ordering Information
SKU229EFDD
UPC662303511142
Model / Product Description95 CU 045X35#SP MIL
Item Weight35.00
Min Order35
Filler Metal Spec Def 
Size.045
Length35 in.
Weight35 lbs., Spool lbs.
PackageSpool