Dual Shield 700X

Designed for flat and horizontal position welding using CO2 shielding gas, Dual Shield 700X provides high deposition rates, high efficiency and excellent performance.

Ordering Information
SKU245019500
UPC662303082208
Model / Product DescriptionDS 700X 1/16X33#AWS
Item Weight33.00
Min Order33
Filler Metal Spec Def 
Size1/16
Length33 in.
Weight33 lbs., Spool lbs.
PackageSpool