Dual Shield 710X

Dual Shield 710X is an all-position flux cored wire that offers outstanding operator appeal with an easily controlled arc, improved operation at both lower and higher current levels, minimal spatter and easily removed slag. It is tested and certified to meet the new AWS A5.20 ‘D’ designation requirements, making this gas-shielded wire an excellent choice for demand critical welds when FEMA 353, D1.1 or D1.8 Seismic Supplement is utilized.

Ordering Information
SKU245019302
UPC662303083489
Model / Product DescriptionDS 710X 1/16X60#CL
Item Weight60.00
Min Order60
Filler Metal Spec Def 
Length60 in.
WeightCoil lbs.