OK Band 308L is a stainless welding strip designed for cladding using the submerged arc welding process. Band 309L together with OK Flux 10.05 and Band 308L produces a 308L deposit.
| SKU | 1161560300 |
|---|---|
| UPC | 662303070601 |
| Model / Product Description | ES OKBAND 11.61X60MMX30KG |
| Item Weight | 66.00 |
| Min Order | 66 |
| Filler Metal Spec Def | |
| Size | 2.36 |
| Weight | 66 lbs. |
| Package | Coil |