Print this page

ESAB MIG-6

ESAB MIG-6 is an ER70S-6 MIG wire suited for welding over heavier amounts of dirt,rust,or mill scale.

Ordering Information
SKU1639C41
UPC662303518530
Model / Product DescriptionMIG-6 052X900#MP
Item Weight900.00
Min Order1800
Filler Metal Spec Def 
Size.052
Weight900 lbs.
PackageMarathon Pack

All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.