ESAB MIG-6 is an ER70S-6 MIG wire suited for welding over heavier amounts of dirt,rust,or mill scale.
| SKU | 163XF41 |
|---|---|
| UPC | 662303668358 |
| Model / Product Description | MIG-6 052X900#OMP PBPLT AB |
| Item Weight | 900.00 |
| Min Order | 1800 |
| Filler Metal Spec Def | |
| Size | .052 |
| Length | 900 in. |
| Weight | 900 lbs., Octagon Marathon Pack lbs. |