OK AristoRod 12.50 is a manganese-silicon alloyed MIG wire used to weld carbon steels. It provides a highly fluid puddle for good wetting action and a high tolerance of rust and mill scale.
| SKU | 1A5011949A |
|---|---|
| UPC | 662303078522 |
| Model / Product Description | OK ARISTOROD12.50 045X900#OMP |
| Item Weight | 900.00 |
| Min Order | 1800 |
| Filler Metal Spec Def | |
| Size | .045 |
| Length | 900 in. |
| Weight | 900 lbs., Octagon Marathon Pack lbs. |
| Package | Octagon Marathon Pack |